Inconel 625 Plates and Sheets Suppliers, Manufacturer & Exporter in Mumbai India.
Introducing Siddhgiri Tube's premium offering: Inconel 625 Plates and Sheets. These plates and sheets are meticulously crafted to meet the highest standards of performance and reliability, particularly in demanding environments. Inconel 625, renowned for its exceptional strength, corrosion resistance, and high-temperature properties, is the material of choice in industries such as aerospace, chemical processing, and marine engineering. Our Inconel 625 Plates and Sheets are engineered with precision and manufactured to the highest standards, ensuring durability, reliability, and versatility. They are designed to withstand
extreme conditions, including high temperatures, pressure variations, and exposure to aggressive chemicals, ensuring the integrity of critical components in various applications. At Siddhgiri Tube, quality is paramount, and our Inconel 625 Plates and Sheets undergo rigorous quality control measures to ensure precision, consistency, and adherence to industry standards. Each plate and sheet is meticulously inspected to guarantee superior quality and customer satisfaction. Partner with Siddhgiri Tube for premium-grade Inconel 625 Plates and Sheets that epitomize innovation, durability, and uncompromising quality. Experience the difference with Siddhgiri Tube, where customer satisfaction is our priority, and excellence is our standard. Trust Siddhgiri Tube to deliver Inconel 625 Plates and Sheets that exceed expectations and set new benchmarks for performance in demanding environments.
Enquire NowSpecifications | : | ASTM / ASME SB 168 |
Size | : | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm |
Thickness | : | 0.1mm to 12 mm Thk |
Form | : | Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange) |
Finish | : | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
Hardness | : | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
Element | Percent by Weight |
---|---|
Carbon | 0.010 maximum |
Manganese | 0.50 maximum |
Phosphorus | 0.015 maximum |
Sulfur | 0.015 maximum |
Silicon | 0.50 maximum |
Chromium | 20.00 – 23.00 |
Nickel | Balance |
Molybdenum | 8.00 – 10.00 |
Columbium | 3.15 – 4.15 |
Titanium | 0.40 maximum |
Aluminum | 0.40 maximum |
Tantalum | 0.05 maximum |
Iron | 5.00 maximum |
Mechanical Properties and Yield Strength of Alloy 625 Plate
Temperature | 0.2% Yield Strength | Ultimate Tensile Strength | Elongation Percent | |||
---|---|---|---|---|---|---|
°F | °C | psi | MPa | psi | MPa |
The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.
Typicals Values at 68°F (20°C)
Yield Strength 0.2% Offset |
Ultimate Tensile Strength |
Elongation in 2 in. |
Hardness | ||
---|---|---|---|---|---|
psi (min.) | (MPa) | psi (min.) | (MPa) | % (min.) | (max.) |
65,000 | 448 | 125,000 | 862 | 50 | 200 Brinell |
STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
Inconel 625 | 2.4856 | N06625 | NCF 625 | NA 21 | ХН75МБТЮ | NC22DNB4MNiCr22Mo9Nb | NiCr23Fe |
Thickness | Thickness | Plate Weight per Unit Area | Density |
---|---|---|---|
3/16 inches | 0.187 inches 4.75 mm | 0.06000 lbs/in² 42.184176 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
1/4 inches | 0.25 inches 6.3500 mm | 0.08 lbs/in² 56.245568 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
3/8 inches | 0.375 inches 9.52 mm | 0.121 lbs/in² 85.0714216 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
1/2 inches | 0.500 inches 12.7 mm | 0.161 lbs/in² 113.1942056 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
5/8 inches | 0.625 inches 15.87 mm | 0.196 lbs/in² 137.8016416 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
3/4 inches | 0.750 inches 19.05 mm | 0.235 lbs/in² 165.221356 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
7/8 inches | 0.875 inches 22.22 mm | 0.274 lbs/in² 192.6410704 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
1 inches | 1.000 inches 25.4 mm | 0.313 lbs/in² 220.0607848 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
1 1/4 inches | 1.250 inches 31.75 mm | 0.391 lbs/in² 274.9002136 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
1 1/2 inches | 1.500 inches 38.1 mm | 0.47 lbs/in² 330.442712 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
1 3/4 inches | 1.750 inches 44.45 mm | 0.549 lbs/in² 385.9852104 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
2 inches | 2.000 inches 50.8 mm | 0.627 lbs/in² 440.8246392 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
2 1/4 inches | 2.250 inches 57.15 mm | 0.705 lbs/in² 495.664068 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
2 1/2 inches | 2.500 inches 63.5 mm | 0.784 lbs/in² 551.2065664 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
2 3/4 inches | 2.75 inches 69.85 mm | 0.862 lbs/in² 606.0459952 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
3 inches | 3.000 inches 76.2 mm | 0.941 lbs/in² 661.5884936 kg/m² | 0.315 lbs/in³ 8.72 g/cm³ |
Inconel 625 Datasheet/ Alloy 625 Data Sheet
Condition | Form | Ultimate Tensile Strength, ksi (MPa) |
Yield Strength at 0.2% offset,ksi (MPa) |
Elongation in 2″ percent |
Hardness, Rockwell |
---|---|---|---|---|---|
Annealed at 1925°F (1052°C), rapid cooled |
Sheet 0.014-0.063″ thick |
132.0 (910) | 67.9 (468) | 47 | B94 |
Annealed at 1925°F (1052°C), rapid cooled |
Sheet,* 0.0.78-0.155″ thick |
131.5 (907) | 67.4 (465) | 45 | B97 |
Annealed at 1925°F (1052°C), rapid cooled |
Plate,*** 1/4″ 1/2″ 3/4″ 1.00″ 1-1/2″ 1-3/4″ |
132.0 (910) 130.0 (896) 132.3 (912) 127.2 (877) 127.3 (878) 128.0 (883) |
65.5 (452) 67.0 (462) 80.0 (552) 75.3 (519) 73.7 (508) 66.0 (455) |
46 44 44 42 43 44 |
B94 B98 B98 B97 B97 C20 |
Aged Hardness, Room Temperature
Form | Aging Temperature, F (C) |
Aging Tme, hrs. | Hardness, Rockwell A |
---|---|---|---|
Plate, 1/2 in. (12.7 mm) thick |
Annealed** | — | 58 |
1200 (649) | 1000 4000 8000 |
68 68 68 |
|
1400 (760) | 1000 4000 8000 |
65 66 65 |
|
1600 (871) | 1000 4000 8000 |
60 60 60 |
Average Tensile Data, Room Temperature
Form | Aging Temperature, F (C) |
Aging Tme, hrs. | Ultimate Tensile Strength, Ksi (MPa) |
Yield Strength at 0.2% offset, Ksi (MPa) |
Elongation in 2 in., (50.8 mm), percent |
---|---|---|---|---|---|
Plate, 1/2 in. (12.7 mm) thick |
Annealed** | — | 127.7 (880) | 66.2 (456) | 46 |
1200 (649) | 1000 4000 8000 16000 |
165.0 (1138) 163.6 (1128) 164.2 (1132) 165.4 (1140) |
122.3 (843) 117.9 (813) 117.8 (812) 118.5 (817) |
28 24 18 12 |
|
1400 (760) | 1000 4000 8000 16000 |
142.9 (985) 145.5 (1003) 142.6 (983) 140.4 (968) |
95.5 (658) 104.1 (718) 97.4 (672) 96.1 (663) |
17 12 13 12 |
|
1600 (871) | 1000 4000 8000 16000 |
130.0 (896) 130.0 (896) 127.0 (876) 128.4 (885) |
68.3 (471) 66.4 (458) 63.7 (439) 63.4 (437) |
30 29 26 32 |
Average Tensile Data, Sheet
Test Temperature, °F(°C) |
Ultimate Tensile Strength, ksi (MPa) |
Yield Strength at 0.2% offset,ksi (MPa) |
Elongation in 2″ percent |
---|---|---|---|
Room 200 400 600 800 1000 1200 1400 1600 1800 2000 |
138.8 (957) 133.3 (919) 129.4 (892) 125.6 (866) 122.2 (843) 119.9 (827) 119.6 (825) 88.4 (609) 52.1 (359) 25.0 (172) 13.3 (92) |
72.0 (496) 67.3 (464) 62.2 (429) 59.5 (410) 59.2 (408) 58.8 (405) 57.0 (393) 55.3 (381) 34.9 (241) 10.8 (75) 6.1 (42) |
38 41 44 45 45 46 47 70 69 108 89 |
Average Rupture Data, Sheet*
Test Temperature, °F(°C) |
Average Rupture Strength, ksi (MPa) for Time Indicated |
||
---|---|---|---|
10 hrs | 100 hrs | 1000 hrs | |
1200 (649) 1400 (760) 1600 (871) |
82 (565) 36 (248) 12 (83) |
71 (490) 27 (186) 6.7 (46) |
60 (414) 20 (138)** 3.7 (26)** |
Temperature Range | Linear Coefficients of Thermal Expansion1 · 10-6 | Thermal Conductivity2 3 | |||
---|---|---|---|---|---|
°C | °F | /°C | /°F | W/m·K | Btu/(hr/ft²/in/°F) |
21 | 70 | 128.9 |
38 | 100 | 129.6 |
93 | 200 | 131.9 |
204 | 400 | 133.9 |
316 | 600 | 134.9 |
427 | 800 | 135.9 |
538 | 1000 | 137.9 |
649 | 1200 | 137.9 |
760 | 1400 | 136.9 |
871 | 1600 | 135.9 |
982 | 1800 | 134.9 |
1093 | 2000 | 133.9 |
Corrosion-resistance of nickel alloys in four 24-hour tests in boiling acetic acid
Alloy | Acetic Acid Concentration |
Corrosion/Erosion Rate | |
---|---|---|---|
mpy | mm/a | ||
Alloy 625 | 10% | 0.39-0.77 | 0.01-0.19 |
Alloy | Corrosion/Erosion Rate | |
---|---|---|
mpy | mm/a | |
Alloy 625 | Nil | Nil |
Pitting resistance equivalency numbers (PREN) for corrosion resistant alloys
Alloy | Ni | Cr | Mo | W | Nb | N | PREN |
---|---|---|---|---|---|---|---|
Alloy 625 | 62 | 22 | 9 | — | 3.5 | — | 40.8 |
Inconel 625 Plates STOCKED SIZES | ||
---|---|---|
SIZE | ALLOY 625 | SIZE |
.125″ | X | 3.18mm |
.134″ | 3.40mm | |
.156″ | X | 3.96mm |
.187″ | X | 4.75mm |
.250″ | X | 6.35mm |
.312″ | X | 7.92mm |
.375″ | X | 9.53mm |
.500″ | X | 12.7mm |
.625″ | X | 15.9mm |
.750″ | X | 19.1mm |
.875″ | 22.2mm | |
1″ | X | 25.4mm |
1.125″ | 28.6mm | |
1.250″ | X | 31.8mm |
1.500″ | X | 38.1mm |
1.750″ | X | 44.5mm |
2″ | X | 50.8mm |
2.500″ | X | 63.5mm |
3″ | 76.2mm |
Bhopal, Lahore, Milan, Hyderabad, Pune, Vadodara, Pimpri-Chinchwad, Aberdeen, Howrah, Jeddah, Riyadh, Bogota, Petaling Jaya, Dallas, Lagos, Nagpur, Houston, Brisbane, Busan, Karachi, Coimbatore, Seoul, Caracas, Atyrau, Perth, Haryana, Bengaluru, Jaipur, Al Jubail, Kuwait City, Al Khobar, Sydney, Ranchi, Chiyoda, Noida, Chandigarh, Secunderabad, Ahvaz, Port-of-Spain, Singapore, Gurgaon, Rajkot, Rio de Janeiro, Abu Dhabi, Hong Kong, Surat, Sharjah, Hanoi, London, Muscat, Jakarta, Navi Mumbai, Istanbul, Kolkata, Cairo, Mumbai, Santiago, Montreal, Faridabad, Vung Tau, Bangkok, Ankara, Ahmedabad, Granada, Melbourne, Tehran, Visakhapatnam, New Delhi, Los Angeles, Ho Chi Minh City, Edmonton, La Victoria, Baroda, Thane, Nashik, Kuala Lumpur, Moscow, Ernakulam, Courbevoie, Calgary, Geoje-si, Indore, New York, Mexico City, Gimhae-si, Ludhiana, Kanpur, Ulsan, Thiruvananthapuram, Manama, Doha, Chennai, Madrid, Jamshedpur, Algiers, Dammam
Iran, Venezuela, Saudi Arabia, Slovakia, Romania, Zimbabwe, Spain, Kazakhstan, Canada, Nigeria, Bulgaria, Afghanistan, Thailand, Bangladesh, Poland, United Kingdom, Bahrain, Jordan, Lithuania, Malaysia, France, Nigeria, Japan, Oman, Lebanon, Germany, Croatia, Australia, Puerto Rico, South Korea, Hungary, United States, Bhutan, Mexico, Mexico, Yemen, Singapore, New Zealand, Ecuador, Gabon, Qatar, Denmark, Iran, Netherlands, Norway, Sri Lanka, Belgium, Libya, Kuwait, Pakistan, Gambia, Sweden, Azerbaijan, Argentina, Chile, Ghana, United Arab Emirates, Finland, Nepal, Trinidad and Tobago,Tunisia, Kenya, Peru, Austria, Russia, Ukraine, Italy, Belarus, Bolivia, Serbia, Poland, Mongolia, Turkey, Czech Republic, South Africa, Angola, India, Vietnam, Indonesia, Tibet, Ireland, Costa Rica, Greece, Colombia, Namibia, Iraq, Estonia, Israel, Macau, Philippines, Brazil, Switzerland, Algeria, Morocco, Chile, Portugal, Egypt, Taiwan, China, Hong Kong.